ASTM B777 Tungsten Heavy Alloy (W-Ni-Fe) Foil & Strip — 90W / 93W / 95W / 97W Grades

ASTM B777 tungsten heavy alloy (W-Ni-Fe) foil and strip is a high-density rolled semi-finished product supplied in the nickel-iron binder family, covering 90W-NiFe, 93W-NiFe, 95W-NiFe, and 97W-NiFe grades (ASTM B777 Class 1 through Class 4, equivalent AMS 7727E / MIL-T-21014). Densities range 16.9 to 18.5 g/cm³ — roughly 1.5–1.7 times lead — with ultimate tensile strengths of 700–980 MPa and hardness HRC 24–32, all in a readily machinable rolled form. Supplied as foil and strip from 0.05 mm to 2.0 mm thickness, widths up to 350 mm, cut-to-length or continuous coil, in the standard sintered → rolled → vacuum stress-relieved condition. W-Ni-Fe grades are magnetic (Ni-Fe binder), which is acceptable for the vast majority of balance-weight, counterweight, inertial, and shielding applications. Typical uses include aircraft and rotor balance weights, gyroscope and accelerometer inertial masses, defense kinetic penetrator components, CT scanner and LINAC collimators, lead-free X-ray/gamma radiation shielding, and oil-and-gas drilling counterweights. Each batch ships with a full Material Test Certificate covering Archimedes density, chemistry, tensile/yield/elongation, HRC hardness, and lot traceability. We supply foil, strip, sheet, and custom-machined parts per drawing as a direct bulk manufacturer, with mill-direct pricing, prototype-to-tonnage lead times, and global delivery to aerospace, defense, medical, and industrial shielding OEMs.

Technical Specifications

PropertyValue
ASTM B777 ClassClass 3 (Magnetic)
Density17.75 – 18.35 g/cm³ (typical 18.0)
Density (lb/in³)~0.65
Melting range~1450–1480°C (solidus; W grains remain solid)
HardnessHRC 27 – 30
Min. Ultimate Tensile Strength≥724 MPa (105 ksi)
Min. Yield Strength (0.2% offset)≥648 MPa (95 ksi)
Elongation≥3% minimum; typically 5–10%
Typical UTS range750 – 950 MPa
Young’s modulus~330 – 350 GPa
Coefficient of thermal expansion~5.5 – 6.5 × 10⁻⁶ /K
Thermal conductivity~120 – 150 W/(m·K)
Magnetic propertyMagnetic (ferromagnetic, due to Ni-Fe binder)
Corrosion resistanceExcellent; superior to lead
ToxicityNon-toxic, lead-free

What Is 95W-NiFe Tungsten Heavy Alloy? Composition and Standard

95W-NiFe is a liquid-phase-sintered tungsten-based composite — a tungsten heavy alloy (WHA) — in which ~95% by volume is sintered tungsten grains bonded by a ductile nickel–iron matrix. It is standardized under ASTM B777 as Class 3 (Magnetic), with cross-references to AMS 7727E Type 2 Class 3 and MIL-T-21014.

Chemical Composition (wt%)

ElementWNiFeImpurities (max)
wt%95.0 ±0.5~3.5~1.5Each ≤0.05
Ni:Fe ratio—≈ 7 : 3——

 

Complete ASTM B777 Tungsten Heavy Alloy Grade Table

ASTM B777 ClassNominal Composition (wt%)Binder SystemMagnetic?Density (g/cm³)Density (lb/in³)Hardness (HRC)Typical UTS (MPa)Typical Elongation
Class 1 (Magnetic)90W – 7Ni – 3FeNi-Fe (7:3)Magnetic16.85 – 17.30~0.6124 – 26700 – 98020 – 33%
Class 1 (Non-Magnetic)90W – 6Ni – 4CuNi-Cu (6:4)Non-Magnetic (μ ≤ 1.05)16.85 – 17.30~0.6124 – 26675 – 85020 – 33%
Class 2 (Magnetic)93W – 5Ni – 2FeNi-Fe (7:3)Magnetic17.15 – 17.85~0.6325 – 27750 – 95010 – 20%
Class 2 (Non-Magnetic)93W – 4Ni – 3CuNi-Cu (≈1:1)Non-Magnetic (μ ≤ 1.05)17.15 – 17.85~0.6325 – 27700 – 90010 – 25%
Class 3 (Magnetic)95W – 3.5Ni – 1.5FeNi-Fe (7:3)Magnetic17.75 – 18.35 ~0.6527 – 30750 – 9505 – 10%
Class 3 (Non-Magnetic)95W – 3.5Ni – 1.5CuNi-Cu (≈7:3)Non-Magnetic (μ ≤ 1.05)17.75 – 18.35~0.6527 – 30720 – 9005 – 15%
Class 4 (Magnetic only)97W – 2.1Ni – 0.9FeNi-Fe (7:3)Magnetic18.25 – 18.85~0.6628 – 32700 – 9003 – 8%

95W-NiFe vs. 90W-NiCu — Which to Choose?

Decision Factor95W-NiFe (Class 3)90W-NiCu (Non-Magnetic, Class 1)
Need maximum density / weight per volume?~18.0 g/cm³17.0 g/cm³ 
Part sits near magnetic sensors / MRI / gyroscopes?Magnetic — will interfereChoose this (μ ≤ 1.05)
Need maximum ductility / formability?Class 3 lower elongationMore ductile (20–33% elongation)
Balance weights in wings / rotors / drilling?Standard choiceUse if magnetic cleanliness required
Radiation shielding near electronics?WorksPrefer non-magnetic if sensors nearby
CostSlightly higher (more W)Slightly lower (less W)

Tungsten Heavy Alloy (W-Ni-Fe) Foil & Strip Application

  • Aerospace balance weights: Aircraft trim weights, control-surface (aileron/elevator/rudder) balance weights, helicopter rotor balancing, turbine and engine counterweights.
  • Inertial navigation & gyroscopes: Precision inertial masses, accelerometer pendulum masses (where magnetic response is acceptable).
  • Defense & ordnance: Kinetic energy penetrator components, missile balance weights, ordnance high-density parts.
  • Medical radiation shielding: CT scanner collimator leaves and bow-tie filters, LINAC multileaf collimators, X-ray shielding sheets, syringe shields.
  • Industrial radiation shielding: Lead-free shielding for NDT, nuclear fuel handling, industrial radiography.
  • Oil & gas: Drill collar counterweights, down-hole balancing hardware.
  • Precision engineering: Scientific instrument weights, clock balances, metrology components.
  • Sports & recreation: Lead-free fishing sinkers, golf club weights.

Frequently Asked Questions

Q: What does 95W-NiFe mean?

A: 95% tungsten by weight, balance (~5%) nickel-iron binder (typical 3.5% Ni + 1.5% Fe). It is the ASTM B777 Class 3 magnetic tungsten heavy alloy grade.

Q: Is 95W-NiFe magnetic?

A: Yes. The nickel-iron binder makes 95W-NiFe ferromagnetic. If you need a non-magnetic grade, choose 90W-NiCu (Class 1 non-magnetic, μ ≤ 1.05) instead.

Q: What is the density of 95W-NiFe?

A: 17.75–18.35 g/cm³, typically ~18.0 g/cm³ — roughly 1.7× the density of lead.

Q: What thicknesses are available?

A: Foil/strip from 0.05 mm to 2.0 mm, width up to 350 mm, cut-to-length or coil. Sheet up to 6 mm and custom-machined parts on request.

Q: Is 95W-NiFe a lead replacement?

A: Yes — it is non-toxic, lead-free, ~1.7× denser than lead, and far stronger and stiffer. It is the standard upgrade for medical shielding and balance weights where lead is restricted.